Customization: | Available |
---|---|
Application: | Communication |
Type: | Single-mode Fiber |
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
The bare fiber of optical fiber is generally divided into three layers: the center high refractive index glass core (the core diameter is generally 50 or 62.5μm), the middle is the low refractive index silica glass cladding (the diameter is generally 125μm), and the outermost is the resin coating for reinforcement. Floor.
Optical fiber specifications:
Single mode: 8/125μm, 9/125μm, 10/125μm
Multimode: 50/125μm, 62.5/125μm
G.652D Single Mode Optical Fiber (B1.3)
|
|||
Item
|
Standard
|
Unit
|
|
Attenuation |
1310nm
|
≤0.35
|
dB/km
|
1383nm
|
≤0.33
|
dB/km
|
|
1550nm
|
≤0.21
|
dB/km
|
|
1625nm
|
≤0.24
|
dB/km
|
|
Dispersion
|
1288nm~1339nm
|
|D|≤3.4
|
ps/(nm·km)
|
1271nm~1360nm
|
|D|≤5.3
|
ps/(nm·km)
|
|
1550nm
|
≤17.8
|
ps/(nm·km)
|
|
Zero-dispersion wavelength
|
1300~1322
|
(nm)
|
|
Zero-dispersion slope
|
≤0.091
|
ps/(nm2•km)
|
|
PMD |
PMD single fiber
|
≤0.15
|
ps/√km
|
PMD Q links
|
≤0.08
|
ps/√km
|
|
MDF
|
1310nm
|
9.2±0.4
|
um
|
Cladding diameter
|
125±1.0
|
μm
|
|
Cladding non-circularity
|
≤0.8
|
%
|
|
Core-cladding concentricity error
|
≤0.6
|
μm
|
|
Coating diameter
|
245±10
|
μm
|
|
Cladding/coating concentricity error
|
≤10.0
|
μm
|
|
Cut-off wavelength
|
1.18~1.33
|
μm
|
|
Macrobend attenuation (ф 50mm, 100 cycles) |
1550nm
|
≤0.05
|
dB
|
1625nm
|
≤0.05
|
dB
|
|
Bending radius
|
≥5
|
m
|
|
Dynamic fatigue parameters
|
≥20
|
nd
|
|
Additional Attenuation @1310nm & @1550nm |
Temperature cycling test:
(-60ºC~85ºC, 3 cycles)
|
≤0.03
|
dB/km
|
Water soak test:
(23ºC for 30 days)
|
≤0.03
|
dB/km
|
|
Damp heat test:
(85ºC, 85%RH for 30 days)
|
≤0.03
|
dB/km
|
|
Thermal aging test (85ºC for 30 days)
|
≤0.03
|
dB/km
|
|
Warm water soak test: (60ºC for 15 days)
|
≤0.03
|
dB/km
|
Optocal Characteristics
|
|||
Item
|
Standard
|
Unit
|
|
Attenuation |
1310nm
|
≤0.35
|
dB/km
|
1383nm
|
≤0.33
|
dB/km
|
|
1550nm
|
≤0.21
|
dB/km
|
|
1625nm
|
≤0.24
|
dB/km
|
|
Attenuation wavelength characteristic 1285nm~1330nm VS 1310nm
1360nm~1410nm VS 1383nm 1525nm~1575nm VS 1550nm |
≤0.03
≤0.05
≤0.02
|
dB/km
|
|
Dispersion |
1288nm~1339nm
|
|D|≤3.4
|
ps/(nm·km)
|
1271nm~1360nm
|
|D|≤6.3
|
ps/(nm·km)
|
|
1550nm
|
≤17.5
|
ps/(nm·km)
|
|
Zero-dispersion wavelength
|
1300~1324
|
(nm)
|
|
Zero-dispersion slope
|
≤0.092
|
ps/(nm2•km)
|
|
PMD |
PMDsingle fiber
|
≤0.15
|
ps/√km
|
PMDQ links
|
≤0.08
|
ps/√km
|
|
cladding diameter
|
125±1.0
|
μm
|
|
Cladding non-circularity
|
≤0.8
|
%
|
|
Core-cladding concentricity error
|
≤0.6
|
μm
|
|
Coating diameter
|
242±7
|
μm
|
|
cladding/coating concentricity error
|
≤10.0
|
μm
|
|
cut-off wavelength
|
1.18~1.33
|
μm
|
|
Macrobend attenuation
(ф 50mm, 100 cycles) |
1550nm(dB)
|
≤0.05
|
dB
|
1625nm(dB)
|
≤0.05
|
dB
|
|
bending radius
|
≥5
|
m
|
|
tensile strength
Wilbur probability level |
≥3.14 (15%)
|
Gpa
|
|
≥3.80 (50%)
|
|||
Dynamic fatigue parameters
|
≥20
|
nd
|
|
Fiber proof-tested
|
1.3≤Fmin-max ≤8.9
|
N
|
|
1.0≤Fave.≤5.0
|
N
|
||
Temperature cycling test: (-60ºC~85ºC,3 cycles)
|
Attenuation @1310nm & @1550nm |
≤0.05
|
dB/km
|
Watersoak test: (23ºC for 30 days)
|
≤0.05
|
dB/km
|
|
Damp heat test: (85ºC,85 for 30 days)
|
≤0.05
|
dB/km
|
|
thermal aging test
(85ºC for 30 days) |
≤0.05
|
dB/km
|
|
Warm water test
(60ºC for 15 days) |
≤0.05
|
dB/km
|